Owing to the extremely low penetration depth of approx. 0.1mm, this method is mainly used for stud welding on thin-walled sheet metals with a thickness of 0.5mm and more. No welding traces are visible on the majority of sheet metals. Even thin sheet metals do not show pressure marks, deformations or discoloration on the reverse side (visible side), even if the surface has been plastic-laminated or electroplated. This method is therefore especially suitable for all stud welding tasks where the decorative appearance of the visible side has to be retained. The ration between minimum sheet tickness and stud diameter amounts to 1 : 10.